S235JR vs. DX51: Understanding the Key Differences in Structural Steels

1. Specification: S235JR and DX51 are both specifications for structural steels. S235JR is a European standard steel grade, while DX51 is a galvanized steel grade.

2. Mechanical composition: The mechanical composition of S235JR includes a minimum yield strength of 235 MPa, a minimum tensile strength of 360-510 MPa, and an elongation of 26%. On the other hand, DX51 has a minimum yield strength of 280 MPa, a minimum tensile strength of 270-500 MPa, and an elongation of 22%.

3. Chemical composition: S235JR has a chemical composition that includes a maximum carbon content of 0.22%, a maximum manganese content of 1.6%, a maximum phosphorus content of 0.05%, and a maximum sulfur content of 0.05%. DX51, being a galvanized steel grade, has a slightly different chemical composition, including a maximum carbon content of 0.12%, a maximum manganese content of 1.7%, a maximum phosphorus content of 0.6%, and a maximum sulfur content of 0.045%.

These key differences in both mechanical and chemical compositions of S235JR and DX51 highlight their distinct properties and applications in various structural projects. It is important to consider these differences to ensure the right material is chosen for specific structural requirements.

da_DKDansk